Structure – dynamic effects in metal melts, glasses and nanocrystals in dependence of temperature
E.D. Kurbanova, V.A. Polukhin
Institute of Metallurgy of the Ural Branch of the Russian Academy of Sciences
DOI: 10.26456/pcascnn/2018.10.414
Abstract: The researchers have conducted a comprehensive analysis of both the original material characteristics and the available information on phase-structural transformations during cooling, glass transition and crystallization of melts, with detailed tracking of their ordering with using the methods as synchrotron X-ray diffraction, scanning electron microscopy, differential scanning calorimetry measurements, and with the interpretation of data by molecular dynamic simulation and thermodynamic calculations.
Keywords: melts, amorphous alloys, glass transition, X-ray diffraction, differential scanning calorimetry, medium order, structural factor, heat capacity, hidden liquid transitions, viscosity, diffusion, crossover.
Bibliography link:
Kurbanova, E.D. Structure – dynamic effects in metal melts, glasses and nanocrystals in dependence of temperature / E.D. Kurbanova, V.A. Polukhin // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2018. – I. 10. – P. 414-419.
Full text (in Russian): download PDF file
Comments are closed.