Contribution of dispersion interaction of s-spheres into the interfacial energy of α – Li and α – Na crystals bounding non-polar organic liquid boundary

I.G. Shebzukhova1, A.M. Apekov2
1Kabardino-Balkarian State University named after H.M. Berbekov
2Institute of Applied Mathematics and Automation KBSC RAS

DOI: 10.26456/pcascnn/2017.9.518

Abstract: The contribution of the dispersion interaction into the interfacial energy of lithium and sodium BCC-crystals has been found on the boundaries with non-polar organic liquids on the grounds of the electron-statistical method as well as the E.M. Lifshits theory.
Keywords: dispersion interaction, interface energy, electron-statistical method, lithium, sodium, non-polar organic liquid, theory by E.M. Lifshits.

Bibliography link:
Shebzukhova, I.G. Contribution of dispersion interaction of s-spheres into the interfacial energy of α – Li and α – Na crystals bounding non-polar organic liquid boundary / I.G. Shebzukhova, A.M. Apekov // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2017. – I. 9. – P. 518-521.