Physical and chemical properties of cement based on calcium phosphate suspensions
O.N. Musskaya, V.K. Krut’ko, A.I. Kulak
Institute of General and Inorganic Chemistry NAS of Belarus
DOI: 10.26456/pcascnn/2017.9.317
Abstract: The effect of phase composition, concentration of calcium phosphates suspensions and polymer binder on the physicochemical properties of calcium phosphate cements is found. It has been established that the introduction of monetite and polymers (polyvinyl alcohol, polyethylene glycol) in the composition of calcium phosphate cements makes it possible to increase their static strength up to 7,1 MPa varying the setting time from 1 min to 1,5 h.
Keywords: calcium phosphate cement, tricalcium phosphate, hydroxyapatite, monetite, polyvinyl alcohol, polyethylene glycol.
Bibliography link:
Musskaya, O.N. Physical and chemical properties of cement based on calcium phosphate suspensions / O.N. Musskaya, V.K. Krut’ko, A.I. Kulak // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2017. – I. 9. – P. 317-322.
Full text (in Russian): download pdf file