Temperature dependence of angles of wetting of porous nickel by Pb-0,49 atomic percent % Na melt

K.M. Elekoeva1, Y.N. Kasumov1, A.R. Manukyants1, M.Kh. Ponegev2, V.A. Sozaev1,2, A.Kh. Shermetov2
1North Caucasian Institute of Mining and Metallurgy (State Technological University)
2Kabardino-Balkarian State University named after H.M. Berbekov

DOI: 10.26456/pcascnn/2017.9.177

Abstract: Polyterms of angles of wetting of porous nickel and nickel of brand НП-2 by  atomic percent  melt are investigated. Thresholds of wetting, which are bound with oxides on the surface of drops and nickel are detected. It is found, that temperature at which the threshold of wetting at porous nickel is observed by ° below than at nickel of brand НП-2.
Keywords: wetting, temperature dependence, porous nickel.

Bibliography link:
Elekoeva, K.M. Temperature dependence of angles of wetting of porous nickel by Pb-0,49 atomic percent % Na melt / K.M. Elekoeva, Y.N. Kasumov, A.R. Manukyants et al. // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2017. – I. 9. – P. 177-181.