Magnetic properties of sintered heterogeneous compositions based on alloys of 3d- and 4f- transition metals

O.B. Dyogteva, Е.М. Semenova, М.B. Lyakhova, Yu.V. Kuznetsova
Tver State University

DOI: 10.26456/pcascnn/2017.9.169

Abstract: The paper presents the results of investigation of the magnetization reversal processes of sintered powder compositions based on micropowders of Nd2Fe14B and Sm(Co0,6Cu0,4)6,0 alloys. Samples were obtained in a high-coercivity state. It is shown that an increase in the volume content of Nd2Fe14B in the composition of the samples under study leads to an increase in the saturation magnetization and to a significant decrease in the coercive force.
Keywords: magnetic properties, heterogeneous state, rare earth intermetallics, coercivity.

Bibliography link:
Dyogteva, O.B. Magnetic properties of sintered heterogeneous compositions based on alloys of 3d- and 4f- transition metals / O.B. Dyogteva, Е.М. Semenova, М.B. Lyakhova, Yu.V. Kuznetsova // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2017. – I. 9. – P. 169-176.

Full text (in Russian): download pdf file

Comments are closed.