Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Structure of rapidly solidified bismuth-tin alloys additional doping with indium

V.G. Shepelevich

DOI: 10.26456/pcascnn/2016.8.404

Original article

Abstract: Results of investigation of phase composition and microstructure of rapidly solidified doping with indium bismuth-tin alloys are presented. Doping with indium causes the consolidation of the structure.

Keywords: high-speed crystallization, foil, specific surface of interphase boundary, tin, bismuth, indium

  • V.G. Shepelevich

For citation:

Shepelevich V.G. Struktura bystrozatverdevshikh splavov vismut-olovo, dopolnitelno legirovannykh indiem [Structure of rapidly solidified bismuth-tin alloys additional doping with indium], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2016, issue 8, pp. 404-409. DOI: 10.26456/pcascnn/2016.8.404.

Full article (in Russian): download PDF file