Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Structural properties of ferroelectric polymers (PVDF and PTFE-42, SKF-32) and composites based on it

R.I. Shakirzyanov, V.A. Astakhov, A.T. Morchenko, N.P. Bessonova, N.A. Shmakova, A.E. Afonkin, A.A. Korlukov, M.I. Buzin

DOI: 10.26456/pcascnn/2016.8.398

Original article

Abstract: Some structural properties of ferroelectric polymer thin film samples of polyvinylidenefluoride, its copolymers (F-42, SKF-32) and its composites with ferrite powder were investigated. Infrared spectroscopy shows that film of SKF-32 does not have areas of VDF chains with long sequences in planar zigzag conformation. Evaluation of the effect of the ferrite particles on the polymer matrix shows, that filler promotes the formation of new crystallization nuclei in the polymer F-42 and PVDF (F2M). By using the methods of polarizing optical microscopy and laser light scattering it was revealed that the PVDF film obtained by hot pressing, have spherilitic supramolecular structure, whereas the samples prepared by precipitation from solution, do not have such structure.

Keywords: ferroelectric polymers, ferrites, composites

  • R.I. Shakirzyanov
  • V.A. Astakhov
  • A.T. Morchenko
  • N.P. Bessonova
  • N.A. Shmakova
  • A.E. Afonkin
  • A.A. Korlukov
  • M.I. Buzin

For citation:

Shakirzyanov R.I., Astakhov V.A., Morchenko A.T., Bessonova N.P., Shmakova N.A., Afonkin A.E., Korlukov A.A., Buzin M.I. Strukturnye svojstva plenok segneto-elektricheskikh polimerov (PVDF i Ftoroplast-42, elastomer SKF-32) i kompozitov na ikh osnove [Structural properties of ferroelectric polymers (PVDF and PTFE-42, SKF-32) and composites based on it], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2016, issue 8, pp. 398-403. DOI: 10.26456/pcascnn/2016.8.398.

Full article (in Russian): download PDF file

Content |