The features of behavior of thermodynamic and structural characteristics of cobalt nanoparticles with «magic» number of atoms

D.N. Sokolov, V.S. Myasnechenko, A.P. Andriychuk, V.V. Kulagin, N.Yu. Sdobnyakov

DOI: 10.26456/pcascnn/2016.8.363

Original article

Abstract: Investigations of thermodynamic and structural characteristics of cobalt nanoclusters in the process of phase transition melting/crystallization with the goal to identify characteristics of their behavior typical for the clusters with the «magic» number of atoms. The melting point of nanoclusters was determined using the temperature dependence of the specific internal energy of nanoclusters.

Keywords: cobalt nanoclusters, phase transition, melting temperature, «magic» numbers

  • D.N. Sokolov
  • V.S. Myasnechenko
  • A.P. Andriychuk
  • V.V. Kulagin
  • N.Yu. Sdobnyakov

For citation:

Sokolov D.N., Myasnechenko V.S., Andriychuk A.P., Kulagin V.V., Sdobnyakov N.Yu. Osobennosti povedeniya termodinamicheskikh i strukturnykh kharakteristik nanochastits kobalta s «magicheskim» chislom atomov [The features of behavior of thermodynamic and structural characteristics of cobalt nanoparticles with «magic» number of atoms], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2016, issue 8, pp. 363-371. DOI: 10.26456/pcascnn/2016.8.363.

Full article (in Russian): download PDF file

Content |