Reliability assessment of composition TiNiHf

P.O. Rusinov, Zh.M. Blednova

DOI: 10.26456/pcascnn/2016.8.315

Original article

Abstract: Based on comprehensive metalophysical researches, new information was obtained aboutthe composition within  the nanoscale surface-modified layer, its structural and mechanical properties. On the basis of experimental data on X-ray analysis of the alloy TiNiHf , the energy consumption, the theoretical strength have been calculated.

Keywords: shape memory effect, mechanical activation, durability, theoretical strength, energy capacity

  • P.O. Rusinov
  • Zh.M. Blednova

For citation:

Rusinov P.O., Blednova Zh.M. Otsenka dolgovechnosti kompozitsii TiNiHf [Reliability assessment of composition TiNiHf], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2016, issue 8, pp. 315-322. DOI: 10.26456/pcascnn/2016.8.315. ⎘