The dependence of the vacancy concentration from the size and shape of the nanocrystal at different pressures

M.N. Magomedov

DOI: 10.26456/pcascnn/2016.8.231

Original article

Abstract: On the basis of generalized RP-model of the nanocrystal, in which there are vacancies in the lattice and the delocalized (diffusing) atoms, the expression for the Helmholtz free energy and the equation of state for the nanocrystal were obtained. The change in the probability of the vacancy formation and the probability of delocalization of an atom, depending on the size and shape of the nanocrystal at different temperatures and pressures were studied. The calculations are performed for BCC iron.

Keywords: vacancies, self-diffusion, nanocrystal, pressure, iron

  • M.N. Magomedov

For citation:

Magomedov M.N. O zavisimosti kontsentratsii vakansij ot razmera i formy nanokristalla pri razlichnykh davleniyakh [The dependence of the vacancy concentration from the size and shape of the nanocrystal at different pressures], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2016, issue 8, pp. 231-238. DOI: 10.26456/pcascnn/2016.8.231.

Full article (in Russian): download PDF file