Effect of penetration depth of exciting electrons on the electron-stimulated desorption yield

Yu.A. Kuznetsov, M.N. Lapushkin

DOI: 10.26456/pcascnn/2016.8.207

Original article

Abstract: We have studied the concentration dependences of electron-stimulated desorption (ESD) of Cs , Na , Sm , and Eu atoms upon their adsorption on nonmetallic layers of films grown on W substrate. It has been found that ESD processes occur at the adlayer – nonmetallic substrate interface.  It has been also shown that reducing the ESD yield beyond one monolayer is due to a decrease in the number of exciting ESD electrons reaching the interface.

Keywords: electron-stimulated desorption, adsorption, alkali metals, rare-earth metals, gold, intermetallic compounds

  • Yu.A. Kuznetsov
  • M.N. Lapushkin

For citation:

Kuznetsov Yu.A., Lapushkin M.N. Vliyanie glubiny proniknoveniya vozbuzhdayushchikh elektronov na vykhod elektronno-stimulirovannoj desorbtsii [Effect of penetration depth of exciting electrons on the electron-stimulated desorption yield], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2016, issue 8, pp. 207-213. DOI: 10.26456/pcascnn/2016.8.207. ⎘

Full article (in Russian): download PDF file