Diffusion processes in nanoscale NaAuy film
M.V. Knatko, M.N. Lapushkin
DOI: 10.26456/pcascnn/2016.8.164
Original article
Abstract: Alkali metal diffusion processes were studied in the semiconductor film NaAuy under the sodium flux modulation conditions deposited on the surface with the following thermal desorption. It is shown that the sodium ion emission in the surface ionization process is determined by a combination of adsorption and diffusion exchanges of Na atoms between surface and volume of the NaAuy film, as well as by diffusion processes within the film.
Keywords: adsorption, alkali metals, gold, intermetallic, thermal desorption of atoms and ions, surface ionization
- M.V. Knatko
- M.N. Lapushkin
For citation:
Knatko M.V., Lapushkin M.N. Diffuzionnye protsessy, protekayushchie v nanorazmernoj plenke NaAu y [Diffusion processes in nanoscale NaAuy film], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2016, issue 8, pp. 164-171. DOI: 10.26456/pcascnn/2016.8.164. ⎘
Full article (in Russian): download PDF file
Content |