Electromasstransport in glasses for electronics

A.M. Karmokov, O.A. Molokanov, Z.V. Shomakhov

DOI: 10.26456/pcascnn/2016.8.151

Original article

Abstract: The results are presented of the investigation of the influence of heating and isothermal exposure on the electrical conductivity special glasses C87-2, C78-4 (lead-silicate) and C78-5 (borate-barium) which are applied in electronics.

Keywords: borate-barium glass, ionic conductivity, crystalline phase, nanoscale phase, annealing, lead-silicate glass, electromasstransport, electrical conductivity, electrical conductivity activation energy

  • A.M. Karmokov
  • O.A. Molokanov
  • Z.V. Shomakhov

For citation:

Karmokov A.M., Molokanov O.A., Shomakhov Z.V. Elektromassoperenos v steklakh dlya elektronnoj tekhniki [Electromasstransport in glasses for electronics], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2016, issue 8, pp. 151-154. DOI: 10.26456/pcascnn/2016.8.151.

Full article (in Russian): download PDF file

Content |