Study of phase formation in the system SrO-Fe2O3-MoO3-B2O3

A.V. Vasiliev, A.G. Fedorovskiy, A.A. Sycheva, L.A. Trusov, E.O. Anokhin, P.E. Kazin

DOI: 10.26456/pcascnn/2016.8.082

Original article

Abstract: Oxide glasses were obtained by high-speed melt quenching. The glass ceramic samples were prepared by thermal crystallization method in reducing atmosphere. The phase composition and magnetic characteristics of the glass-containing Sr2FeMoO3 are investigated.

Keywords: strontium hexaferrite, magnetic nanoparticles, magnetic fluids, colloids, colloidal stability

  • A.V. Vasiliev
  • A.G. Fedorovskiy
  • A.A. Sycheva
  • L.A. Trusov
  • E.O. Anokhin
  • P.E. Kazin

For citation:

Vasiliev A.V., Fedorovskiy A.G., Sycheva A.A., Trusov L.A., Anokhin E.O., Kazin P.E. Izuchenie fazoobrazovaniya v sisteme SrO – Fe2O3 – MoO3 – B2O3 [Study of phase formation in the system SrO-Fe2O3-MoO3-B2O3], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2016, issue 8, pp. 82-87. DOI: 10.26456/pcascnn/2016.8.082.

Full article (in Russian): download PDF file

Content |