Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


The synthesis of composites based on powders of aluminium with small additions of barium

S.A. Bibanaeva, V.M. Skachkov, B.N. Latosh, N.A. Sabirzyanov

DOI: 10.26456/pcascnn/2016.8.059

Original article

Abstract: The article describes a method of producing a porous material of aluminum powders doped with small additions of barium after treatment with water. Studies of the strength properties, microstructure, specific surface area of the original samples and derived products were performed.

Keywords: aluminium powder, barium, cermet, specific surface, microhardness, scanning microscopy

  • S.A. Bibanaeva
  • V.M. Skachkov
  • B.N. Latosh
  • N.A. Sabirzyanov

For citation:

Bibanaeva S.A., Skachkov V.M., Latosh B.N., Sabirzyanov N.A. Sintez poristykh materialov na osnove poroshkov alyuminiya s malymi dobavkami bariya [The synthesis of composites based on powders of aluminium with small additions of barium], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2016, issue 8, pp. 59-63. DOI: 10.26456/pcascnn/2016.8.059.

Full article (in Russian): download PDF file

Content |