SYNTHESIS AND STUDYING OF ACID-BASE PROPERTIES OF TiO -Ag 2 NANOCOMPOSITE

M.S. Shama, A.A. Kravtsov, A.V. Blinov, M.A. Jasnaja, D.G. Selemeneva

DOI: 10.26456/pcascnn/2015.7.519

Original article

Abstract: This article is devoted to studying the acid-base properties of the surface of titanium dioxide and Ag nanocomposite based on it (TiOmodified nanosize silver) synthesized by sol-gel method.

Keywords: TiO2 nanoparticles, nanocomposite TiO – Ag 2 , the sol-gel method, acid-base properties, the indicating method

  • M.S. Shama
  • A.A. Kravtsov
  • A.V. Blinov
  • M.A. Jasnaja
  • D.G. Selemeneva

For citation:

Shama M.S., Kravtsov A.A., Blinov A.V., Jasnaja M.A., Selemeneva D.G. Sintez i issledovanie kislotno-osnovnykh svojstv nanokompozita TiO2 – Ag [SYNTHESIS AND STUDYING OF ACID-BASE PROPERTIES OF TiO -Ag 2 NANOCOMPOSITE], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2015, issue 7, pp. 519-526. DOI: 10.26456/pcascnn/2015.7.519.

Full article (in Russian): download PDF file

Content |