INVESTIGATION OF THE FORMATION PROCESSES OF URANIUM AND ALUMINUM OXIDES NANOCLUSTERS ON THE SURFACE OF OXIDIZED ALUMNUM USING DOUBLE LASER PULSES
D.S. Umreiko, A.I. Komyak, E.V. Vileishikova, A.P. Zajogin
DOI: 10.26456/pcascnn/2015.7.505
Original article
Abstract: This work presents the results obtained in studies of the production of variable valence uranium oxides at the surface of oxidized aluminum under irradiation by double laser pulses. The well developed aluminum surface activated by uranium oxides was produced with the use of a LSS-1 multichannel laser atomic-emission spectrometer with double pulses.
Keywords: spectral analysis, uranium complexes, laser atomic-emission spectrometry, double laser pulses
- D.S. Umreiko
- A.I. Komyak
- E.V. Vileishikova
- A.P. Zajogin
For citation:
Umreiko D.S., Komyak A.I., Vileishikova E.V., Zajogin A.P. Issledovanie protsessov obrazovaniya nanoklasterov oksidov urana i alyuminiya na poverkhnosti oksidirovannogo alyuminiya sdvoennymi lazernymi impulsami [INVESTIGATION OF THE FORMATION PROCESSES OF URANIUM AND ALUMINUM OXIDES NANOCLUSTERS ON THE SURFACE OF OXIDIZED ALUMNUM USING DOUBLE LASER PULSES], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2015, issue 7, pp. 505-508. DOI: 10.26456/pcascnn/2015.7.505. ⎘
Full article (in Russian): download PDF file
Content |