Phenomenological description of vitrification and structural relaxation processes
Yu.K. Startsev
DOI: 10.26456/pcascnn/2015.7.494
Original article
Abstract: Analysis of characteristics of relaxation processes of vitrification and their known phenomenological descriptions was done. A detailed examination of the microscopic description of vitrification and nature of atomic dynamics in glassy materials led the author to the conclusion that physical-chemical functions of fractional exponents, widely used for the spectrum of structural relaxation times.
Keywords: glassy state, relaxation processes, stretched exponent
- Yu.K. Startsev
For citation:
Startsev Yu.K. Fenomenologicheskoe opisanie steklovaniya i protsessov strukturnoj relaksatsii [Phenomenological description of vitrification and structural relaxation processes], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2015, issue 7, pp. 494-504. DOI: 10.26456/pcascnn/2015.7.494. ⎘
Full article (in Russian): download PDF file
Content |