EFFECT OF SOLID COMPONENT OF DIFFUSION-HARDENING SOLDERS ON PROPERTIES OF CONNECTING LAYER

V.M. Skachkov, S.P. Yatsenko, L.A. Pasechnik, N.A. Sabirzyanov

DOI: 10.26456/pcascnn/2015.7.463

Original article

Abstract: The article provides new formulations of gallium-based composite alloys. The influence of the composition of powder filler on the structure and properties of solder for the purpose of obtaining unique properties and expansion of areas of their use is investigated.

Keywords: diffusion-hardening composite alloys, solders, filler, structure, properties

  • V.M. Skachkov
  • S.P. Yatsenko
  • L.A. Pasechnik
  • N.A. Sabirzyanov

For citation:

Skachkov V.M., Yatsenko S.P., Pasechnik L.A., Sabirzyanov N.A. Vliyanie tverdoj komponenty diffuzionno-tverdeyushchikh pripoev na svojstva soedinitelnogo sloya [EFFECT OF SOLID COMPONENT OF DIFFUSION-HARDENING SOLDERS ON PROPERTIES OF CONNECTING LAYER], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2015, issue 7, pp. 463-470. DOI: 10.26456/pcascnn/2015.7.463.

Full article (in Russian): download PDF file

Content |