INFLUENCE OF CALCINATION TEMPERATURE ON STRUCTURAL CHANGES OF NANOSIZED ZIRCONIA

D.G. Selemeneva, A.A. Kravtsov, A.V. Blinov, M.A. Jasnaja

DOI: 10.26456/pcascnn/2015.7.450

Original article

Abstract: The synthesis of nanosized zirconia by sol-gel method was performed. The optimal conditions for stable ZrOgel was determined, and then was set a point of gelation. Obtained samples of zirconia nanoparticles were studied by infrared spectroscopy and XRD analysis. Acid-base properties of the surface of the samples were studied by indicator method.

Keywords: sol-gel method, ZrO2 nanoparticles, infrared spectroscopy, X-ray difraction analysis, indicator method

  • D.G. Selemeneva
  • A.A. Kravtsov
  • A.V. Blinov
  • M.A. Jasnaja

For citation:

Selemeneva D.G., Kravtsov A.A., Blinov A.V., Jasnaja M.A. Vliyanie temperatury prokalivaniya na strukturnye izmeneniya nanorazmernogo dioksida tsirkoniya [INFLUENCE OF CALCINATION TEMPERATURE ON STRUCTURAL CHANGES OF NANOSIZED ZIRCONIA], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2015, issue 7, pp. 450-455. DOI: 10.26456/pcascnn/2015.7.450.

Full article (in Russian): download PDF file

Content |