ON ALTERNATIVE APPROACHES TO DETERMINATION OF RADIUS AND OTHER GEOMETRIC CHARACTERISTICS OF NANOPARTICLES

V.M. Samsonov

DOI: 10.26456/pcascnn/2015.7.413

Original article

Abstract: The concept of the nanoparticle radius has been analysed and its relationship with the number of molecules (atoms) the particle consists of. A conclusion has been made that in most cases the radius of the equimolecular dividing surface can be used as an adequate measure of the particle size.

Keywords: nanoparticle, radius, equimolecular dividing surface, nanoclusters, Gibbs method of surface phases, Wigner-Seitz radius, gyroscopic radius

  • V.M. Samsonov

For citation:

Samsonov V.M. Ob alternativnykh podkhodakh k opredeleniyu radiusa i drugikh geometricheskikh kharakteristik nanochastits [ON ALTERNATIVE APPROACHES TO DETERMINATION OF RADIUS AND OTHER GEOMETRIC CHARACTERISTICS OF NANOPARTICLES], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2015, issue 7, pp. 413-424. DOI: 10.26456/pcascnn/2015.7.413.

Full article (in Russian): download PDF file

Content |