DISCRETE MODELING AT THE ATOMIC-MOLECULAR LEVEL OF MECHANICAL PROCESSES IN NANOCOMPOSITES
V.I. Repchenkov, Y.E. Nagorny, A.V. Akavity
DOI: 10.26456/pcascnn/2015.7.400
Original article
Abstract: An analysis of the quadratic force fields at the interfaces in composites is presented.
Keywords: composite materials, carbon nanotubes, covalent bonds, non-bonded connection, interface, normal and tangential stresses
- V.I. Repchenkov
- Y.E. Nagorny
- A.V. Akavity
For citation:
Repchenkov V.I., Nagorny Y.E., Akavity A.V. Diskretnoe modelirovanie na atomno-molekulyarnom urovne mekhanicheskikh protsessov v nanokompozitakh [DISCRETE MODELING AT THE ATOMIC-MOLECULAR LEVEL OF MECHANICAL PROCESSES IN NANOCOMPOSITES], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2015, issue 7, pp. 400-406. DOI: 10.26456/pcascnn/2015.7.400. ⎘