THE PROCESSES OF OBTAINING «COMPLEX» FILMS ON ALUMINUM

E.S. Markaryan

DOI: 10.26456/pcascnn/2015.7.367

Original article

Abstract: In this paper, we consider the processes occurring during the formation of «complex» films on aluminum. We prepared them according to the characteristic of the growth kinetics of a continuous film in a matrix of porous anodic oxide. The geometric parameters of the nanostructured aluminum oxide were obtained in the process of reanodizing.

Keywords: anodic aluminum oxide, growth kinetics, «complex film», growth rate, porosity

  • E.S. Markaryan

For citation:

Markaryan E.S. Issledovanie protsessov polucheniya «kompleksnykh» plenok na alyuminii [THE PROCESSES OF OBTAINING «COMPLEX» FILMS ON ALUMINUM], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2015, issue 7, pp. 367-377. DOI: 10.26456/pcascnn/2015.7.367.

Full article (in Russian): download PDF file

Content |