Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


THE DEVELOPMENT OF CORSEGRAINED MODEL OF ALUMINOSILICATE HALLOYSITE NANOTUBES

P.V. Komarov, V.A. Ivanov

DOI: 10.26456/pcascnn/2015.7.302

Original article

Abstract: The problems of constructing of large-scale model of composites based on polymers and aluminosilicate nanotubes have been considered.

Keywords: nanocomposite, nanoparticles, computer simulation

  • P.V. Komarov
  • V.A. Ivanov

For citation:

Komarov P.V., Ivanov V.A. Razrabotka krupnozernistoj modeli alyumosilikatnykh nanotrubok galluazita [THE DEVELOPMENT OF CORSEGRAINED MODEL OF ALUMINOSILICATE HALLOYSITE NANOTUBES], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2015, issue 7, pp. 302-310. DOI: 10.26456/pcascnn/2015.7.302.