THE ELECTRO-PHYSICAL PROPERTIES OF A SPECIAL GLASS ELECTRONIC ENGINEERINGS
A.M. Karmokov, O.A. Molokanov, Z.V. Shomakhov
DOI: 10.26456/pcascnn/2015.7.263
Original article
Abstract: The regularities of changes in the electrical properties of glasses S87-2, S78-4, S78-5 used in vacuum electronics. A correlation between structural change and electrical conductivity is proposed. A comparative analysis was carried out of the influence of an electric current on the formation of a new phase and the time to reach the phase equilibrium in the glass.
Keywords: microchannel plate, the emission layer, lead-silicate glass, barium borate glass, conductivity, isothermal annealing, elektromassoperenos, phase equilibria
- A.M. Karmokov
- O.A. Molokanov
- Z.V. Shomakhov
For citation:
Karmokov A.M., Molokanov O.A., Shomakhov Z.V. Elektrofizicheskie svojstva spetsialnykh stekol elektronnoj tekhniki [THE ELECTRO-PHYSICAL PROPERTIES OF A SPECIAL GLASS ELECTRONIC ENGINEERINGS], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2015, issue 7, pp. 263-269. DOI: 10.26456/pcascnn/2015.7.263. ⎘
Full article (in Russian): download PDF file
Content |