PROPERTIES OF ZnO CERAMICS SINTERED FROM NANOPOWDERS ZnO-Zn , OBTAINED PULSED ELECTRON EVAPORATION
V.G. Il`ves, S.Yu. Sokovnin, V.R. Khrustov, S.V. Zayats, S.V. Pryanichnikov, M.G. Zuev
DOI: 10.26456/pcascnn/2015.7.249
Original article
Abstract: We investigated the properties of ceramic ZnO, sintered from nanopowders ZnO–Zn, obtained by a pulsed electron evaporation of diverse targets. Behavior of shrinkage curves of nano ZnO–Zn depends on the history of their production. Evolution of properties of nanoparticles ZnO–Zn during annealing in the air were traced via XRD and pulsed cathodoluminescence.
Keywords: pulsed electron beam, nanopowders ZnO–Zn, ceramic ZnO–Zn, cathodoluminescence ceramic ZnO–Zn
- V.G. Il`ves
- S.Yu. Sokovnin
- V.R. Khrustov
- S.V. Zayats
- S.V. Pryanichnikov
- M.G. Zuev
For citation:
Il`ves V.G., Sokovnin S.Yu., Khrustov V.R., Zayats S.V., Pryanichnikov S.V., Zuev M.G. Svojstva keramiki ZnO , spechennoj iz nanoporoshkov ZnO – Zn , poluchennykh impulsnym elektronnym ispareniem [PROPERTIES OF ZnO CERAMICS SINTERED FROM NANOPOWDERS ZnO-Zn , OBTAINED PULSED ELECTRON EVAPORATION], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2015, issue 7, pp. 249-256. DOI: 10.26456/pcascnn/2015.7.249. ⎘
Full article (in Russian): download PDF file
Content |