THE INFLUENCE OF THIN FATTY ACID FILMS ON TRIBOLOGICAL PROPERTIES OF A DISCRETE CONTACT OF METAL SURFACES

V.V. Izmailov, A.F. Gusev, M.V. Novoselova

DOI: 10.26456/pcascnn/2015.7.242

Original article

Abstract: The values of the coefficient of friction in a single ball–plane contact have been measured experimentally under small normal loads (0,5 – 5 mN). The contact parts are made of steel. The experiments have been carried out with thin fatty acid films layered on a flat contact part. The fatty acids have various molecular lengths. Experimentally obtained values of the specific force of friction at a microscale level are higher than similar values known from literature and obtained in experiments at a macroscale level.

Keywords: friction coefficient, specific force of friction, fatty acids

  • V.V. Izmailov
  • A.F. Gusev
  • M.V. Novoselova

For citation:

Izmailov V.V., Gusev A.F., Novoselova M.V. Vliyanie tonkikh plyonok zhirnykh kislot na tribologicheskie svojstva diskretnogo kontakta metallicheskikh poverkhnostej [THE INFLUENCE OF THIN FATTY ACID FILMS ON TRIBOLOGICAL PROPERTIES OF A DISCRETE CONTACT OF METAL SURFACES], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2015, issue 7, pp. 242-248. DOI: 10.26456/pcascnn/2015.7.242.

Full article (in Russian): download PDF file

Content |