SEM STUDY OF THE MICROSTRUCTURE OF BIOCOMPOSITES BASED ON HIGHLY POROUS HONEYCOMB MATERIALS

I.G. Grigorov, A.G. Shirokova, E.A. Bogdanova, V.M. Skachkov, S.V. Borisov, N.A. Sabirzyanov

DOI: 10.26456/pcascnn/2015.7.179

Original article

Abstract: The paper is devoted to the study of the morphology and surface topography of the synthesized biocomposites, intended for creation of implants by scanning electron microscopy. Produced by ion-plasma spraying NiTi was selected as the metal substrate. Bioactive coating formed from an aqueous slurry of hydroxyapatite. The effectiveness of the proposed in the work methods of the coating was evaluated by constructing 2D- and 3D-images of the surface.

Keywords: implant, biocomposites, Titanium Nickelide ( NiTi ), hydroxyapatite (HAP), 2D-, 3Dimage, scanning electron microscopy

  • I.G. Grigorov
  • A.G. Shirokova
  • E.A. Bogdanova
  • V.M. Skachkov
  • S.V. Borisov
  • N.A. Sabirzyanov

For citation:

Grigorov I.G., Shirokova A.G., Bogdanova E.A., Skachkov V.M., Borisov S.V., Sabirzyanov N.A. Issledovanie mikrostruktury biokompozitov na osnove vysokoporistykh yacheistykh materialov metodami skaniruyushchej elektronnoj mikroskopii [SEM STUDY OF THE MICROSTRUCTURE OF BIOCOMPOSITES BASED ON HIGHLY POROUS HONEYCOMB MATERIALS], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2015, issue 7, pp. 179-185. DOI: 10.26456/pcascnn/2015.7.179.

Full article (in Russian): download PDF file

Content |