INFLUENCE OF TEMPERATURE TREATMENT ON THE STRUCTURE AND COMPOSITION OF NANOSIZED ZnO, OBTAINED BY SOL-GEL METHOD
A.V. Blinov, A.A. Kravtsov, M.A. Jasnaja, A.Yu. Rusanov, E.V. Momot
DOI: 10.26456/pcascnn/2015.7.123
Original article
Abstract: Synthesis of nano-sized zinc oxide was performed by sol-gel method. The structure of the nano-sized ZnO was studied at the gel stage. The effect of calcination temperature on ZnO nanoparticles size and polydispersity of the samples and their phase composition and structure was investigated. IR spectroscopy of the samples of nano-sized zinc oxide was carried out.
Keywords: ZnO nanoparticles, sol-gel method, TEM, XRD, IR spectroscopy
- A.V. Blinov
- A.A. Kravtsov
- M.A. Jasnaja
- A.Yu. Rusanov
- E.V. Momot
For citation:
Blinov A.V., Kravtsov A.A., Jasnaja M.A., Rusanov A.Yu., Momot E.V. Vliyanie temperaturnoj obrabotki na strukturu i sostav nanorazmernogo ZnO, poluchennogo zol-gel metodom [INFLUENCE OF TEMPERATURE TREATMENT ON THE STRUCTURE AND COMPOSITION OF NANOSIZED ZnO, OBTAINED BY SOL-GEL METHOD], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2015, issue 7, pp. 123-129. DOI: 10.26456/pcascnn/2015.7.123. ⎘
Full article (in Russian): download PDF file
Content |