INFLUENCE OF SODIUM CHLORIDE BARRIER ON THE SIZE AND PARTICLE MORPHOLOGY OF SYNTHESIZED COBALT OXIDE

A.Sh.. Khaliullina, V.G. Vassil'ev, E.V. Vladimirova, V.I. Pastukhove, T.S. Karpova, E.S. Gerasimova

DOI: 10.26456/pcascnn/2014.6.424

Original article

Abstract: Powders of cobalt oxide consisting from different size and morphology particles have been obtained by methods of thermal hydrolysis, thermal hydrolysis with sodium chloride as a barrier and thermal decomposition of cobalt oxalate. The size and morphology of the particles in obtained powders were investigated to the dependence of synthesis method.

Keywords: thermohydrolisis, barrier, sodium chloride, cobalt oxalate, cobalt oxide, nanoparticles, morphology

  • A.Sh.. Khaliullina
  • V.G. Vassil'ev
  • E.V. Vladimirova
  • V.I. Pastukhove
  • T.S. Karpova
  • E.S. Gerasimova

For citation:

Khaliullina A.Sh.., Vassil'ev V.G., Vladimirova E.V., Pastukhove V.I., Karpova T.S., Gerasimova E.S. Vliyanie khloridno-natrievogo barera na razmer i morfologiyu chastits sinteziruemogo oksida kobalta [INFLUENCE OF SODIUM CHLORIDE BARRIER ON THE SIZE AND PARTICLE MORPHOLOGY OF SYNTHESIZED COBALT OXIDE], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2014, issue 6, pp. 424-429. DOI: 10.26456/pcascnn/2014.6.424. ⎘

Full article (in Russian): download PDF file

⇐ Prevoius journal article | Content | Next journal article ⇒