BULK AND SURFACE NANOSTRUCTURING OF TITANIUM BASED ALLOYS

V.V. Stolyarov

DOI: 10.26456/pcascnn/2014.6.379

Original article

Abstract: The paper is a brief review of structure refinement deformation methods for bulk samples of titanium alloys with different nature. Typical microstructures of alloys in nanostructured and ultrafine-grained state are demonstrated.

Keywords: microstructure, deformation, rolling, pressing, forging

  • V.V. Stolyarov

For citation:

Stolyarov V.V. Obemnoe i poverkhnostnoe nanostrukturirovanie titanovykh splavov [BULK AND SURFACE NANOSTRUCTURING OF TITANIUM BASED ALLOYS], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2014, issue 6, pp. 379-389. DOI: 10.26456/pcascnn/2014.6.379.