EFFECT OF THE STRUCTURE AND SYMMETRY ON THE THERMODYNAMIC PROPERTIES OF NANOPARTICLES WITH THE «MAGIC» NUMBER OF ATOMS
N.Yu.. Sdobnyakov, V.S. Myasnichenko, A.P. Andriychuk, D.N. Sokolov
DOI: 10.26456/pcascnn/2014.6.362
Original article
Abstract: The investigation of the thermodynamic characteristics of the gold nanoclusters with «magic» numbers of atoms in melting/crystallization phase transition has been carried out. Using the temperature dependence of the specific internal energy of nanoclusters, the melting temperature has been determined.
Keywords: nanoclusters, phase transition, melting temperature, «magic» numbers
- N.Yu.. Sdobnyakov
- V.S. Myasnichenko
- A.P. Andriychuk
- D.N. Sokolov
For citation:
Sdobnyakov N.Yu.., Myasnichenko V.S., Andriychuk A.P., Sokolov D.N. Vliyanie struktury i simmetrii na termodinamicheskie svojstva nanochastits s «magicheskim» chislom atomov [EFFECT OF THE STRUCTURE AND SYMMETRY ON THE THERMODYNAMIC PROPERTIES OF NANOPARTICLES WITH THE «MAGIC» NUMBER OF ATOMS], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2014, issue 6, pp. 362-369. DOI: 10.26456/pcascnn/2014.6.362. ⎘
Full article (in Russian): download PDF file
⇐ Prevoius journal article | Content | Next journal article ⇒