САLCULATION OF THE HEAT OF FUSION AND THE HEAT OF FREEZING SIZE DEPENDENCIES FOR METAL NANOPARTICLES

N.Yu.. Sdobnyakov, D.N. Sokolov, V.S. Myasnichenko, A.N. Bazulev

DOI: 10.26456/pcascnn/2014.6.342

Original article

Abstract: On the basis of temperature dependencies of internal energy the size dependences of heat of fusion and heat of freezing for gold, cuprum, aluminum and cobalt nanoclusters have been calculated. For the simulation the Monte-Carlo method has been used and interaction between atoms has been described by many-body Gupta potential.

Keywords: heat of fusion, heat of freezing, Monte-Carlo method, Gupta potential, metal nanoclusters

  • N.Yu.. Sdobnyakov
  • D.N. Sokolov
  • V.S. Myasnichenko
  • A.N. Bazulev

For citation:

Sdobnyakov N.Yu.., Sokolov D.N., Myasnichenko V.S., Bazulev A.N. Raschet razmernykh zavisimostej teplot plavleniya i kristallizatsii nanochastits metallov [САLCULATION OF THE HEAT OF FUSION AND THE HEAT OF FREEZING SIZE DEPENDENCIES FOR METAL NANOPARTICLES], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2014, issue 6, pp. 342-348. DOI: 10.26456/pcascnn/2014.6.342.

Full article (in Russian): download PDF file

⇐ Prevoius journal article | Content | Next journal article ⇒