CALCULATION OF STRESS-STRAIN STATE OF STRETCHING NANOTUBES WITH DEFECTS
Y.E. Nagorny, A.V. Akavity, V.I. Repchenkov
DOI: 10.26456/pcascnn/2014.6.273
Original article
Abstract: This paper presents the results of numerical calculation and analysis of the stress-strain state of a regular straight single-walled open carbon nanotube with vacancies in tension.
Keywords: carbon nanotubes, defects, vacancies, stress-strain state
- Y.E. Nagorny
- A.V. Akavity
- V.I. Repchenkov
For citation:
Nagorny Y.E., Akavity A.V., Repchenkov V.I. Raschet napryazhenno-deformirovannogo sostoyaniya uglerodnykh nanotrubok s defektami pri rastyazhenii [CALCULATION OF STRESS-STRAIN STATE OF STRETCHING NANOTUBES WITH DEFECTS], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2014, issue 6, pp. 273-279. DOI: 10.26456/pcascnn/2014.6.273. ⎘
Full article (in Russian): download PDF file
⇐ Prevoius journal article | Content | Next journal article ⇒