FRACTAL ANALYSIS OF PHOTOINDICED LIGHT SCATTERING PICTURES IN LiNbO3 CRYSTALS

D.V. Manukovskaya, N.V. Sidorov, M.N. Palatnikov, O.R. Starodub

DOI: 10.26456/pcascnn/2014.6.247

Original article

Abstract: The dynamics of laser-induced defects in different layers of photoinduced light scattering (PILS) pictures in lithium niobate was researched by analysis of fractal dimension of PILS picture layers. Stoichiometric LiNbO3 crystal had different genesis. This method was compared with the method of measurement of PILS indicatrix opening angle. The transition of energy between PILS layers was detected.

Keywords: lithium niobate, photoinduced light scattering, laser-induced defects, fractal dimension

  • D.V. Manukovskaya
  • N.V. Sidorov
  • M.N. Palatnikov
  • O.R. Starodub

For citation:

Manukovskaya D.V., Sidorov N.V., Palatnikov M.N., Starodub O.R. Fraktalnyj analiz kartin fotoindutsirovannogo rasseyaniya sveta v kristallakh LiNbO3 [FRACTAL ANALYSIS OF PHOTOINDICED LIGHT SCATTERING PICTURES IN LiNbO3 CRYSTALS], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2014, issue 6, pp. 247-252. DOI: 10.26456/pcascnn/2014.6.247.

Full article (in Russian): download PDF file

Content |