ON THE DEPENDENCIES OF THE COEFFICIENT OF THERMAL EXPANSION VERSUS SIZE AND SHAPE OF NANOCRYSTAL

M.N. Magomedov

DOI: 10.26456/pcascnn/2014.6.239

Original article

Abstract: A model of nanocrystal in the form of a rectangular parallelepiped with a variable surface shape (RP-model) is used to study of the dependencies of the coefficient of thermal expansion (αp) versus size and surface shape of the nanocrystal of the simple matter. The calculations for the nanocrystal of silicon have shown that α increases at reduction N, moreover at reduction of the temperature the dependency αp (N) is increasing. At the isomorphous reduction N along isotherm of 100K the function αp (N) at defined size (for cube N ≅1125) passes from the negative into the positive field.

Keywords: nanocrystal, size, shape of the surfaces, thermal expansion

  • M.N. Magomedov

For citation:

Magomedov M.N. O zavisimosti koeffitsienta teplovogo rasshireniya ot razmera i formy nanokristalla [ON THE DEPENDENCIES OF THE COEFFICIENT OF THERMAL EXPANSION VERSUS SIZE AND SHAPE OF NANOCRYSTAL], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2014, issue 6, pp. 239-246. DOI: 10.26456/pcascnn/2014.6.239.

Full article (in Russian): download PDF file

⇐ Prevoius journal article | Content | Next journal article ⇒