A STATIONARY THERMAL LENS RESPONSE OF A NANOLIQUID
A.I. Livashvily, G.D. Ivanova, V.K. Khe
DOI: 10.26456/pcascnn/2014.6.227
Original article
Abstract: The stationary two-dimensional thermodiffusion in a two component medium in the Gaussian beam radiation field was analyzed. The expression for a thermo-lens medium response is obtained.
Keywords: thermal lens, thermodiffusion, two components medium
- A.I. Livashvily
- G.D. Ivanova
- V.K. Khe
For citation:
Livashvily A.I., Ivanova G.D., Khe V.K. Statsionarnyj termolinzovyj otklik nanozhidkosti [A STATIONARY THERMAL LENS RESPONSE OF A NANOLIQUID], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2014, issue 6, pp. 227-230. DOI: 10.26456/pcascnn/2014.6.227. ⎘