ELECTRON-STIMULATED OXIDATION OF THE SURFACE POLYCRYSTALLINE THALLIUM

D.A. Krimshokalova, I.B. Ashkhotova, O.G. Ashkhotov

DOI: 10.26456/pcascnn/2014.6.220

Original article

Abstract: In this paper, using Auger electron spectroscopy and electron energy-loss spectroscopy the kinetics of oxygen adsorption on thallium was studied in two cases: under continuous electron irradiation (100-1000 eV) and without depending on the exposure time in oxygen at a partial pressure oxygen 10−6 Torr at room temperature.

Keywords: exposure, electrons, energy, spectroscopy, surface oxidation kinetics, radiation, adsorption, concentration, monolayer, thallium

  • D.A. Krimshokalova
  • I.B. Ashkhotova
  • O.G. Ashkhotov

For citation:

Krimshokalova D.A., Ashkhotova I.B., Ashkhotov O.G. Elektronno-stimulirovannoe okislenie poverkhnosti polikristallicheskogo talliya [ELECTRON-STIMULATED OXIDATION OF THE SURFACE POLYCRYSTALLINE THALLIUM], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2014, issue 6, pp. 220-226. DOI: 10.26456/pcascnn/2014.6.220.

Full article (in Russian): download PDF file

⇐ Prevoius journal article | Content | Next journal article ⇒