EFFECT OF SURFACE CHEMISTRY OF NANODIAMOND FILLER ON THE PROPERTIES OF POLYTETRAFLUOROETHYLENE COMPOSITES
A.P. Koscheev, A.A. Perov, P.V. Gorokhov, A.V. Tereshenkov, N.A. Chukov, S.A. Khatipov
DOI: 10.26456/pcascnn/2014.6.208
Original article
Abstract: The tribology properties of polymer composites of polytetrafluoroethylene filled with detonation nanodiamonds of various types were studied. The composite properties were found to depend on the oxygen-containing groups on nanodiamond surface. The direct evidence of chemical interaction of nanodiamond with polymer matrix during preparation (sintering stage) of composite was obtained.
Keywords: polytetrafluoroethylene composites, nanodiamond, surface chemistry, thermodesorption mass spectrometry
- A.P. Koscheev
- A.A. Perov
- P.V. Gorokhov
- A.V. Tereshenkov
- N.A. Chukov
- S.A. Khatipov
For citation:
Koscheev A.P., Perov A.A., Gorokhov P.V., Tereshenkov A.V., Chukov N.A., Khatipov S.A. Vliyanie khimii poverkhnosti nanoalmaznogo napolnitelya na svojstva kompozitov na osnove politetraftoretilena [EFFECT OF SURFACE CHEMISTRY OF NANODIAMOND FILLER ON THE PROPERTIES OF POLYTETRAFLUOROETHYLENE COMPOSITES], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2014, issue 6, pp. 208-213. DOI: 10.26456/pcascnn/2014.6.208. ⎘
Full article (in Russian): download PDF file
⇐ Prevoius journal article | Content | Next journal article ⇒