THERMAL DECOMPOSITION OF POLYMER COMPOSITE OF POLYTETRAFLUOROETHYLENE AND DETONATION NANODIAMONDS

A.P. Koscheev, P.V. Gorokhov, A.A. Perov, S.A. Khatipov

DOI: 10.26456/pcascnn/2014.6.202

Original article

Abstract: The effect of nanodiamond filler on the thermal decomposition of polytetrafluoroethylene composites under vacuum pyrolysis was studied by means of thermodesoption mass spectrometry. The results indicate that the presence of nanodiamonds affects both the temperature profiles and the chemical composition of decomposition products.

Keywords: polytetrafluoroethylene composites, detonation nanodiamond, thermal destruction, thermodesorption mass spectrometry

  • A.P. Koscheev
  • P.V. Gorokhov
  • A.A. Perov
  • S.A. Khatipov

For citation:

Koscheev A.P., Gorokhov P.V., Perov A.A., Khatipov S.A. Termodestruktsiya polimernogo kompozita na osnove politetraftoretilena i detonatsionnykh nanoalmazov [THERMAL DECOMPOSITION OF POLYMER COMPOSITE OF POLYTETRAFLUOROETHYLENE AND DETONATION NANODIAMONDS], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2014, issue 6, pp. 202-207. DOI: 10.26456/pcascnn/2014.6.202.

Full article (in Russian): download PDF file

⇐ Prevoius journal article | Content | Next journal article ⇒