DETERMINE THE OPTIMUM PARAMETERS OF THE SYSTEM FOR CREATING GOLD NANOSCALE CONTACTS BETWEEN TRACKS OF NANOSCALE BUSES
A.Yu.. Kolosov, D.N. Sokolov, N.Yu.. Sdobnyakov, M.A. Kharitonova
DOI: 10.26456/pcascnn/2014.6.193
Original article
Abstract: The simulation of the creating gold nanoscale contacts between tracks of nanoscale buses for different system configurations by Monte-Carlo method was carried out. The interaction between nanoparticles was described by many-body Gupta potential. The optimum parameters for creating nanoscale contacts between tracks of nanoscale buses have been determined. The final stable structure of nanoscale contacts has been analyzed.
Keywords: nanoscale contact, gold nanoparticles, coalescence, Monte-Carlo method, Gupta potential, phase transition, stability
- A.Yu.. Kolosov
- D.N. Sokolov
- N.Yu.. Sdobnyakov
- M.A. Kharitonova
For citation:
Kolosov A.Yu.., Sokolov D.N., Sdobnyakov N.Yu.., Kharitonova M.A. Opredelenie optimalnykh parametrov sistemy dlya formirovaniya nanokontaktov zolota mezhdu dorozhkami nanorazmernoj shiny [DETERMINE THE OPTIMUM PARAMETERS OF THE SYSTEM FOR CREATING GOLD NANOSCALE CONTACTS BETWEEN TRACKS OF NANOSCALE BUSES], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2014, issue 6, pp. 193-201. DOI: 10.26456/pcascnn/2014.6.193. ⎘
Full article (in Russian): download PDF file