SIZE EFFECT OF TEMPERATURE ON CONTACT MELTING OF SMALL- DIMENSIONAL PHASES

O.V. Gudieva, D.A. Kambolov, P.K. Korotkov, V.A. Sozaev

DOI: 10.26456/pcascnn/2014.6.101

Original article

Abstract: The attempt to derive the relation for the temperature of contact melting of small-dimensional phases (nanoparticles, nanofilms) has been made with account for the A.I. Rusanov size dependence of the surface tension of nanoparticles.

Keywords: size effect, surface energy, temperature of contact melting, nanofilms, nanoparticles, nanowires

  • O.V. Gudieva
  • D.A. Kambolov
  • P.K. Korotkov
  • V.A. Sozaev

For citation:

Gudieva O.V., Kambolov D.A., Korotkov P.K., Sozaev V.A. Razmernyj effekt temperatury kontaktnogo plavleniya nizkorazmernykh faz [SIZE EFFECT OF TEMPERATURE ON CONTACT MELTING OF SMALL- DIMENSIONAL PHASES], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2014, issue 6, pp. 101-104. DOI: 10.26456/pcascnn/2014.6.101.

Full article (in Russian): download PDF file

⇐ Prevoius journal article | Content | Next journal article ⇒