E.N. Gribanov, O.I. Markov, Yu..V. Khripunov
DOI: 10.26456/pcascnn/2014.6.095
Original article
Abstract: In this paper results of calculations by quantum-chemical methods of structure and power parameters of nanoclusters of bismuth-antimony Bi8 , Bi7Sb1 , Bi6Sb2 , Bi5Sb3 , Bi4Sb4 . Bi3Sb5 , Bi2Sb6 , Bi1Sb7 , Sb8 are presented.
Keywords: cluster, bismuth, antimony semiconductor – semimetal transition
- E.N. Gribanov
- O.I. Markov
- Yu..V. Khripunov
For citation:
Gribanov E.N., Markov O.I., Khripunov Yu..V. Modelirovanie klasterov Bi8-nSbn [MODELING OF CLUSTERS Bi8-nSbn], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2014, issue 6, pp. 95-100. DOI: 10.26456/pcascnn/2014.6.095. ⎘