Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


FORMATION OF HYBRID CARBON sp2 AND sp3 PHASES FROM GRAPHENE LAYERS L4-8

E.A. Belenkov, M.I. Tingaev

DOI: 10.26456/pcascnn/2014.6.041

Original article

Abstract: In this paper research of carbon compounds is connected, which can be obtained as a result of partial cross-linking of graphene layers L4−8 . It is established that after cross-linking and geometry optimization of graphene layers L4−8 only diamond-like phase or the original graphene layers L4−8 can be obtained.

Keywords: carbon, diamond, graphene, crystalline structure

  • E.A. Belenkov
  • M.I. Tingaev

For citation:

Belenkov E.A., Tingaev M.I. Poluchenie gibridnykh uglerodnykh sp2 i sp3 faz iz sloev grafena L4-8 [FORMATION OF HYBRID CARBON sp2 AND sp3 PHASES FROM GRAPHENE LAYERS L4-8], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2014, issue 6, pp. 41-46. DOI: 10.26456/pcascnn/2014.6.041. ⎘

Full article (in Russian): download PDF file

Content |